Section 33.1-14-03-05 - Lap seam crack
Universal Citation: ND Admin Code ยง 33.1-14-03-05
Current through Supplement No. 394, October, 2024
The shell or drum of a boiler in which a lap seam crack is discovered along a longitudinal riveted joint must be immediately discontinued from use. If the boiler is not more than fifteen years of age, a complete new course of the original thickness may be installed at the discretion of the chief inspector. Patching is prohibited. "Lap seam crack" means the typical crack frequently found in lap seams, extending parallel to the longitudinal joint and located either between or adjacent to rivet holes.
General Authority: NDCC 23.1-16
Law Implemented: NDCC 23.1-16
Disclaimer: These regulations may not be the most recent version. North Dakota may have more current or accurate information. We make no warranties or guarantees about the accuracy, completeness, or adequacy of the information contained on this site or the information linked to on the state site. Please check official sources.
This site is protected by reCAPTCHA and the Google
Privacy Policy and
Terms of Service apply.