Illinois Administrative Code
Title 35 - ENVIRONMENTAL PROTECTION
Part 223 - STANDARDS AND LIMITATIONS FOR ORGANIC MATERIAL EMISSIONS FOR AREA SOURCES
Subpart C - ARCHITECTURAL AND INDUSTRIAL MAINTENANCE COATINGS
Section 223.310 - Standards

Current through Register Vol. 48, No. 38, September 20, 2024

a) VOM Content Limits: Except as provided in subsection (c), no person shall manufacture, blend, or repackage for sale within Illinois, supply, sell, or offer for sale within Illinois, or solicit for application or apply within Illinois, any architectural coating manufactured on or after July 1, 2009 that contains a VOM content in excess of the corresponding limit specified below:

VOM Content Limit

Grams/Liter

(Pounds/Gallon)

Coating Category

1)

Flat Coatings

100

(0.8)

2)

Non-Flat Coatings

150

(1.3 )

3)

Non-Flat High-Gloss Coatings

250

(2.1)

Specialty Coatings

4)

Antenna Coatings

530

(4.4)

5)

Antifouling Coatings

400

(3.3)

6)

Bituminous Roof Coatings

300

(2.5)

7)

Bituminous Roof Primers

350

(2.9)

8)

Bond Breakers

350

(2.9)

9)

Calcamine Recoaters

475

(4.0)

10)

Clear Wood Coatings

A)

Clear Brushing Lacquers

680

(5.7)

B)

Lacquers

(including lacquer sanding sealers)

550

(4.6)

C)

Sanding Sealers

(other than lacquer sanding sealers)

350

(2.9)

D)

Varnishes

350

(2.9)

11)

Concrete Curing Compounds

350

(2.9)

Concrete Surface Retarder

780

(6.5)

12)

Conversion Varnish

725

(6.0)

13)

Dry Fog Coatings

400

(3.3)

14)

Faux Finishing Coatings

350

(2.9)

15)

Fire-Resistive Coatings

350

(2.9)

16)

Fire-Retardant Coatings

A)

Clear

650

(5.4)

B)

Opaque

350

(2.9)

17)

Floor Coatings

250

(2.1)

18)

Flow Coatings

420

(3.5)

19)

Form-Release Compounds

250

(2.1)

20)

Graphic Arts Coatings (Sign Paints)

500

(4.2)

21)

High-Temperature Coatings

420

(3.5)

22)

Impacted Immersion Coating

780

(6.5)

23)

Industrial Maintenance Coatings

340

(2.8)

24)

Low-Solids Coatings

120

(1.0)

25)

Magnesite Cement Coatings

450

(3.8)

26)

Mastic Texture Coatings

300

(2.5)

27)

Metallic Pigmented Coatings

500

(4.2)

28)

Multi-Color Coatings

250

(2.1)

29)

Nuclear Coating

450

(3.8)

30)

Pre-Treatment Wash Primers

420

(3.5)

31)

Primers, Sealers, and Undercoaters

200

(1.7)

32)

Quick-Dry Enamels

250

(2.1)

33)

Quick-Dry Primers, Sealers and Undercoaters

200

(1.7)

34)

Recycled Coatings

250

(2.1)

35)

Roof Coatings

250

(2.1)

36)

Rust Preventive Coatings

400

(3.3)

37)

Shellacs

A)

Clear

730

(6.1)

B)

Opaque

550

(4.6)

38)

Specialty Primers, Sealers, and Undercoaters

350

(2.9)

39)

Stains

250

(2.1)

40)

Stone Consolidants

450

(3.8)

41)

Swimming Pool Coatings

340

(2.8)

42)

Swimming Pool Repair and Maintenance Coatings

340

(2.8)

43)

Temperature-Indicator Safety Coatings

550

(4.6)

44)

Thermoplastic Rubber Coatings and Mastics

550

(4.6)

45)

Traffic Marking Coatings

150

(1.3)

46)

Waterproofing Concrete/Masonry Sealers

400

(3.3)

47)

Waterproofing Sealers

250

(2.1)

48)

Wood Preservatives

350

(2.9)

BOARD NOTE: Conversion factor: one pound VOM per gallon (U.S.) = 119.95 grams per liter.

b) Limits are expressed in grams of VOM per liter of coating thinned to the manufacturer's maximum recommendation, excluding the volume of any water, exempt compounds, or colorant added to tint bases. "Manufacturers maximum recommendation" means the maximum recommendation for thinning that is indicated on the label or lid of the coating container.

c) Most Restrictive VOM Limit. If anywhere on the container of any architectural coating, or any label or sticker affixed to the container, or in any sales, advertising, or technical literature supplied by a manufacturer or anyone acting on the manufacturer's behalf, any representation is made that indicates that the coating meets the definition of or is recommended for use for more than one of the coating categories listed in subsection (a), then the most restrictive VOM content limit shall apply. This provision does not apply to the coating categories specified in subsections (c)(1) through (c)(21):

1) Lacquer coatings (including lacquer sanding sealers);

2) Metallic pigmented coatings;

3) Shellacs;

4) Fire-retardant coatings;

5) Pretreatment wash primers;

6) Industrial maintenance coatings;

7) Low-solids coatings;

8) Wood preservatives;

9) High-temperature coatings;

10) Temperature-indicator safety coatings;

11) Antenna coatings;

12) Antifouling coatings;

13) Flow coatings;

14) Bituminous roof primers;

15) Specialty primers, sealers, and undercoaters;

16) Conversion varnish;

17) Calcimine recoaters;

18) Impacted immersion coatings;

19) Nuclear coatings;

20) Thermoplastic rubber coating and mastics;

21) Concrete surface retarder.

d) Painting Practices. All architectural coating containers used to apply their contents to a surface directly from the container by pouring, siphoning, brushing, rolling, padding, ragging, or other means shall be closed when not in use. These architectural coatings containers include, but are not limited to, drums, buckets, cans, pails, trays, or other application containers. Containers of any VOM-containing materials used for thinning and cleanup shall also be closed when not in use.

e) Thinning. No person who applies or solicits the application of any architectural coating shall apply a coating that is thinned to exceed the applicable VOM limit specified in subsection (a).

f) Rust Preventive Coatings. No person shall apply or solicit the application of any rust preventive coating for industrial use unless the rust preventive coating complies with the industrial maintenance coating VOM limit specified in subsection (a). If the coating is also regulated under another Part, the more restrictive limit shall apply.

g) Coatings Not Listed in Subsection (a). For any coating that does not meet any of the definitions for the specialty coatings categories listed in subsection (a), the VOM content limit shall be determined by classifying the coating as a flat coating, a non-flat coating, or a non-flat high-gloss coating, based on its gloss, as defined in Section 223.307, and the corresponding flat or non-flat coating limit shall apply.

Disclaimer: These regulations may not be the most recent version. Illinois may have more current or accurate information. We make no warranties or guarantees about the accuracy, completeness, or adequacy of the information contained on this site or the information linked to on the state site. Please check official sources.