Hawaii Administrative Rules
Title 6 - DEPARTMENT OF BUDGET AND FINANCE
Division - PUBLIC UTILITIES COMMISSION
Chapter 77 - TRANSPORTATION OF NATURAL AND OTHER GAS BY PIPELINE; MINIMUM SAFETY STANDARDS
Subchapter 11 - MINIMUM SAFETY STANDARDS - REQUIREMENTS FOR CORROSION CONTROL
Section 6-77-140 - Remedial measures: distribution lines other than cast iron or ductile iron lines

Universal Citation: HI Admin Rules 6-77-140

Current through August, 2024

(a) General corrosion. Except for cast iron or ductile iron pipe, each segment of generally corroded distribution line pipe with a remaining wall thickness less than that required for the maximum allowable operating pressure of the pipeline, or a remaining wall thickness less than thirty percent of the nominal wall thickness, must be replaced. However, if the area of general corrosion is small, the corroded pipe may be repaired. Corrosion pitting so closely grouped as to affect the overall strength of the pipe is considered general corrosion for the purpose of this subsection.

(b) Localized corrosion pitting. Except for cast iron or ductile iron pipe, each segment of distribution line pipe with localized corrosion pitting to a degree where leakage might result must be replaced or repaired.

Disclaimer: These regulations may not be the most recent version. Hawaii may have more current or accurate information. We make no warranties or guarantees about the accuracy, completeness, or adequacy of the information contained on this site or the information linked to on the state site. Please check official sources.